Mechanical Properties Metric English Comments
Charpy Impact Unnotched 24.0 J/cm²

@Temperature -30.0 °C
114 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p..
Charpy Impact Unnotched 24.0 J/cm²

@Temperature -40.0 °C
114 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Charpy Impact Unnotched 24.0 J/cm²

@Temperature -30.0 °C
114 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2640 E4 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF
Charpy Impact Unnotched 24.0 J/cm²

@Temperature -30.0 °C
114 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2650 Z6 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF
Charpy Impact Unnotched 24.0 J/cm²

@Temperature -30.0 °C
114 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2650 Z6 POM + PUR
Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF