Polymer Property : Charpy Impact Unnotched = 20.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -20.0 °C
20.9 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 66 HI/1 PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -20.0 °C
20.9 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 25 E LS PA6 reinforced with glass fiber, UV stabilized
PA 6 grade for extrusion, reinforced with 25% glass fiber, determined for extrusion of window profile systems. Delivered in natural as well as full RAL scale color.Information Provided by Plastcom s..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -20.0 °C
20.9 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 25 FRC 4 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 25 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability according to UL 94 3 at 1,6mm, glow wire at 960°C. Applic..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Cycoloy® C4215HF PC+ABS (Europe-Africa-Middle East)
Cycoloy C4215HF is a 15% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic apprearance. It combines good processability with a low s..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RV150 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S RV150 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F2K4 Nylon 6, Glass Fiber/Bead Filled
SAXAMID 126F2K4 is a 10% glass fibers and 20% glass beads filled polyamide 6 injection-molding-grade.Information provided by SAX Polymers
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® S RV300AE (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..