Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold release. Vydyne R633H has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption, and part weight are key advantages of Vydyne glass-reinforced PA66/6 resins over aluminum and/or zinc die cast parts. Vydyne R633H is specially formulated to minimize the oxidative and thermal degradation of the PA666/6 copolymer when exposed to elevated temperatures for extended periods of time. Product provides improved retention of physical properties under exposure to long term heat. Vydyne R633H provides a higher heat distortion temperature, better resistance to creep, higher impact and better dimensional stability compared with unreinforced PA66/6. This product also provides a combination of excellent surface appearance with high tensile and modulus properties. This property balance enables usage of Vydyne R633H in applications where aesthetics and performance are important. Typical Applications/End Uses: Vydyne R633H resin has been used for many under-the-hood automotive applications, motor housings for power tools, and garden appliances. These resins have also been used in miscellaneous brackets, gears and clips that require high rigidity and strength. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 33% Filler by WeightAdditive:LubricantHeat Stabilizer Features:CopolymerGood Mold ReleaseGood Surface FinishHeat Stabilized High Tensile Strength Lubricated Uses:Automotive Under the HoodGearsHousingsLawn and Garden EquipmentMetal ReplacementPower/Other ToolsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Water Absorption 1.3 %

@Time 86400 sec
1.3 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Diameter 2.00 mm
0.0040 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Diameter 2.00 mm
0.0090 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 184 MPa
26700 psi
ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 10.8 GPa
1570 ksi
ISO 527-2
Flexural Strength 255 MPa
37000 psi
ISO 178
Flexural Modulus 8.80 GPa
1280 ksi
ISO 178
Poissons Ratio 0.40
0.40
ISO 527-2
Izod Impact, Notched (ISO) 12.0 kJ/m²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 180
13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 1.50 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
0.833 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 10.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
5.56 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 260 °C
500 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 230 °C
446 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Unannealed; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Nozzle Temperature 280 - 310 °C
536 - 590 °F
Melt Temperature 285 - 305 °C
545 - 581 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Suggested Max Regrind 25 %
Users viewing this material also viewed the following: