Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® EQ 18 N Polyethylene
Impact modified PE for extrusion. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C...
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc
FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PP EIP5025 F VT2 Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE
Information provided by Polykemi AB
Charpy Impact Unnotched 1.20 - 1.40 J/cm²

@Temperature 23.0 °C
5.71 - 6.66 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 59 T 40 LW 031 PP, 40% mineral filling, laser label
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc.Contains modificator for laser labeling of finisched parts. /LASER NdIAG..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..