Plastcom PLASTALEN® EQ 18 N Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTALEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTALEN® EQ 18 N Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified PE for extrusion. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.880 g/cc
0.0318 lb/in³
STN EN ISO 1183-1
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
STN EN ISO 527-2
Elongation at Break 80 %
80 %
STN EN ISO 527-2
Tensile Modulus 0.750 GPa
109 ksi
STN EN ISO 527-2
Flexural Strength 24.0 MPa
3480 psi
STN EN ISO 178
Flexural Modulus 0.800 GPa
116 ksi
STN EN ISO 178
Charpy Impact Unnotched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
STN EN ISO 75-2 (A)
Vicat Softening Point 94.0 °C
201 °F
STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 650 °C

@Thickness 3.00 mm
1200 °F

@Thickness 0.118 in
STN EN 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 170 - 220 °C
338 - 428 °F
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved