Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 12 T 30 TS PP reinforced with 30% mineral filler Features: Modified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in t.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in the.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 71 T 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrin.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 32 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 52 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 63 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 152 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – vegetable boxes for refrigerators, shower enclosure panels, CD and DVD cases. Blends with.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Solvay TECHNYL® A 246M PA66, DRY Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 73 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Charpy Impact Unnotched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 172 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS.. |