Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.80 J/cm² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Novamid® 1013GMF H2 NAT/BK37 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding, Excellent Dimensional Stability |
|||
Charpy Impact Unnotched | 7.80 J/cm² @Temperature -30.0 °C |
37.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Charpy Impact Unnotched | 7.80 J/cm² @Temperature -30.0 °C |
37.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |