Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 80.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature 23.0 °C
80.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Novodur® E401 ABS
Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution
Charpy Impact Unnotched 17.0 J/cm²

@Temperature 23.0 °C
80.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Terluran® HD-15 ABS
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 17.0 J/cm²

@Temperature 23.0 °C
80.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis Daplen™ EE158AI Polypropylene TPO Compound
Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® S1320 003 POM
Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature 23.0 °C
80.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® S1320 003 POM
Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® S2320 003 POM
Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® S2320 003 PRO BK 00120 POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® S2320 003 PRO POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t..
Copyright © lookpolymers.com All Rights Reserved