Mechanical Properties Metric English Comments
Adhesive Bond Strength 27.6 MPa

@Temperature 25.0 °C
4000 psi

@Temperature 77.0 °F
Tensile Lap Shear
Henkel Hysol EA 9321 Paste Adhesive System
Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair
Adhesive Bond Strength 27.6 MPa

@Temperature -55.0 °C
4000 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9359.3 Paste Adhesive System
Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding
Adhesive Bond Strength 27.6 MPa

@Temperature -55.0 °C
4000 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9360 Paste Adhesive System
Structural adhesive, exhibits excellent peel strength, tensile lap shear strength.Applications: Structural Repair Composite Bonding Liquid Shim
Adhesive Bond Strength 27.6 MPa

@Temperature 25.0 °C
4000 psi

@Temperature 77.0 °F
Tensile Lap Shear
Henkel Hysol EA 9395 Paste Adhesive System
Two-part, nonmetallic-filled version of Hysol EA 9394.Applications: Potting Structural Repair Composite Bonding