Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 27.6 MPa @Temperature 25.0 °C |
4000 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |
|||
Adhesive Bond Strength | 27.6 MPa @Temperature -55.0 °C |
4000 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9359.3 Paste Adhesive System Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding |
|||
Adhesive Bond Strength | 27.6 MPa @Temperature -55.0 °C |
4000 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9360 Paste Adhesive System Structural adhesive, exhibits excellent peel strength, tensile lap shear strength.Applications: Structural Repair Composite Bonding Liquid Shim |
|||
Adhesive Bond Strength | 27.6 MPa @Temperature 25.0 °C |
4000 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9395 Paste Adhesive System Two-part, nonmetallic-filled version of Hysol EA 9394.Applications: Potting Structural Repair Composite Bonding |