Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 35.0 - 67.0 kJ/m²

@Temperature -30.0 - -30.0 °C
16.7 - 31.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 52.8 kJ/m² Grade Count:5
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Unnotched (ISO) 55.0 - 67.0 kJ/m²

@Temperature -30.0 - -30.0 °C
26.2 - 31.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 61.0 kJ/m² Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..