Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 35.0 - 67.0 kJ/m² @Temperature -30.0 - -30.0 °C |
16.7 - 31.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 52.8 kJ/m² Grade Count:5 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 - 67.0 kJ/m² @Temperature -30.0 - -30.0 °C |
26.2 - 31.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 61.0 kJ/m² Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |