Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 87.0 kJ/m²
41.4 ft-lb/in²
ISO 180
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where ..
Izod Impact, Unnotched (ISO) 87.0 kJ/m²
41.4 ft-lb/in²
ISO 180
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..
Izod Impact, Unnotched (ISO) 87.0 kJ/m²

@Temperature 23.0 °C
41.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon TD000
LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 87.0 kJ/m²
41.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON TD000 PU
LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 87.0 kJ/m²

@Temperature 23.0 °C
41.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East)
LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Izod Impact, Unnotched (ISO) 87.0 kJ/m²

@Temperature 23.0 °C
41.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11
LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 87.0 kJ/m²
41.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized.
Izod Impact, Unnotched (ISO) 87.0 kJ/m²

@Temperature -30.0 °C
41.4 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 180/1U
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..