Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS (Asia Pacific)
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP KONDUIT MT00E PP
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific)
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East)
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 7.00 kJ/m² - NB
3.33 ft-lb/in² - NB
Average value: 10.2 kJ/m² Grade Count:6
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
DIN 53453
Ineos Nova S-6600MG Compact Polystyrene Microgranulates  (discontinued **)
High impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm especially useful for compounding and extrusion applications. Due to the higher viscosity intensive mixing with thermoplas..
Izod Impact, Unnotched (ISO) 7.00 kJ/m² - NB

@Temperature -40.0 - -30.0 °C
3.33 ft-lb/in² - NB

@Temperature -40.0 - -22.0 °F
Average value: 66.2 kJ/m² Grade Count:25
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp CI001 PS
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America..
Izod Impact, Unnotched (ISO) 7.00 - 90.0 kJ/m²
3.33 - 42.8 ft-lb/in²
Average value: 60.9 kJ/m² Grade Count:31
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
SYNTHOS Krasten® 137 General Purpose Polystyrene
Easy flow. Examples of Application:Injection moulding – cups and containers for the food industry, medical devices, drawing templates.Extrusion – coextrusion, high gloss surface.Synthos wa..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
SYNTHOS Krasten® 154 General Purpose Polystyrene
Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS
LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific)
LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Europe-Africa-Middle East)
LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp FF008L PE
LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1U
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY
Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.Available in: Europe and North AmericaProduct Applications: TECHNYL® AR 218 V25 BLACK..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1C
Chi Mei Polyrex® PG-33 Polystyrene
Standard grade
Izod Impact, Unnotched (ISO) 7.00 - 11.0 kJ/m²
3.33 - 5.23 ft-lb/in²
Spec; ISO 180
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene
PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co..
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1U
A.D. Compound Adene NCTA Homopolymer 50% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Unnotched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..