Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Bead Filled
Manufacturer Addiplast
Trade Name Addinyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Conditioned; ISO 868
87
87
ISO 868
Tensile Strength at Break 60.0 MPa
8700 psi
Conditioned; ISO R 527
80.0 MPa
11600 psi
ISO R 527
Elongation at Yield 7.0 %
7.0 %
ISO R 527
11 %
11 %
Conditioned; ISO R 527
Modulus of Elasticity 1.80 GPa
261 ksi
Conditioned; ISO 178
3.80 GPa
551 ksi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/1A
7.00 kJ/m²
3.33 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179/IeU
6.00 J/cm²
28.6 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/IeA
0.500 J/cm²
2.38 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
ASTM E831
Melting Point 260 °C
500 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
Conditioned; CEI 60243-1
30.0 kV/mm
762 kV/in
CEI 60243-1
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A