Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH 7059 Polypropylene, Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Total Atofina
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 7059 Polypropylene, Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning properties and optimal thermal bonding performance. PPH 7059 has a special anti gas-fading formulation to reduce yellowing in fibers.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ISO 2039-2
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-2
Flexural Modulus 1.50 GPa
218 ksi
ISO 527-2
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C per hour; ISO 75-2
Vicat Softening Point 87.0 °C
189 °F
50N-50°C per hour; ISO 306
152 °C
306 °F
10N-50°C per hour; ISO 306