Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 27.3 kJ/m² | 13.0 ft-lb/in² | ISO 180/A |
ExxonMobil Exxtral™ BMV 208 Performance Polyolefin Product Description: Polyolefin injection molding compound with very high flow, high stiffness, good low temperature impact resistance, and excellent processability for automotive exterior trim appl.. |
|||
Izod Impact, Notched (ISO) | 27.3 kJ/m² | 13.0 ft-lb/in² | Partial Break; ISO 180 |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |
|||
Izod Impact, Notched (ISO) | 27.3 kJ/m² | 13.0 ft-lb/in² | ASTM D-256 |
Bapolene® 5005H High Density Polyethylene This resin is a high molecular weight, high density copolymer polyethylene resin. Product exhibits superior impact strength and ESCR. Applications: Drums and Industrial Parts.Bapolene® and Bapolan.. |