Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) SH-0150 Acrylonitrile Butadiene Styrene SH - 0150 ABS extrusion grade has been formulated to provide excellent mechanical properties,extrusion stability, vacuum formability and chemical resistance. It is a high flow extrusion grade with h.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
MRC Polymers MAXTEL™ 600T18 TPO, 18% Talc Filled • For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation pr.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
MRC Polymers MAXTEL™ 600T18-UV TPO, 18% Talc Filled, UV Stabilized • For automotive exterior applications• Excellent process ability and dimensional stabilityInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180-1A |
Gromax BTG25-FN09N1 Nylon 6 25% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, Conditioned Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP YF003S Polyester Elastomer (Europe-Africa-Middle East) LNP* THERMOCOMP* YF003S is a compound based on Polyester Elastomer containing Glass Fiber. Added features include; Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Izod Impact, Notched (ISO) | >= 28.0 kJ/m² | >= 13.3 ft-lb/in² | |
Styrolution Absolac® 200 ABS Electroplating gradeInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL ENV150 PPE (Europe-Africa-Middle East) Noryl* ENV150 modified polyphenylene ether resin is an unfilled, flame retardant high heat grade suitable for extrusion molding conversion route. It uses non-chlorinated, non-brominated FR additives.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature -50.0 °C |
13.3 ft-lb/in² @Temperature -58.0 °F |
|
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
13.3 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
80*10*4; ISO 180/1A |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |