MRC Polymers MAXTELâ„¢ 600T18 TPO, 18% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer MRC Polymers
Trade Name MAXTEL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers MAXTELâ„¢ 600T18 TPO, 18% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ISO 1183
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Flexural Strength 22.0 MPa
3190 psi
ISO 178
Flexural Modulus 1.15 GPa
167 ksi
ISO 178
Izod Impact, Notched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75