Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.02 - 1.20 g/cc
0.0368 - 0.0434 lb/in³
Average value: 1.05 g/cc Grade Count:101
Water Absorption 0.250 - 1.00 %
0.250 - 1.00 %
Average value: 0.448 % Grade Count:24
Moisture Absorption at Equilibrium 0.000 - 0.210 %
0.000 - 0.210 %
Average value: 0.176 % Grade Count:8
Water Absorption at Saturation 0.300 - 1.00 %
0.300 - 1.00 %
Average value: 0.738 % Grade Count:4
Maximum Moisture Content 0.0100 - 0.150
0.0100 - 0.150
Average value: 0.0256 Grade Count:9
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cm
0.00200 - 0.00800 in/in
Average value: 0.00530 cm/cm Grade Count:54
Melt Flow 0.100 - 35.0 g/10 min
0.100 - 35.0 g/10 min
Average value: 4.93 g/10 min Grade Count:103
Mechanical Properties Metric English Comments
Hardness, Rockwell R 68.0 - 113
68.0 - 113
Average value: 102 Grade Count:55
Ball Indentation Hardness 65.0 - 105 MPa
9430 - 15200 psi
Average value: 90.0 MPa Grade Count:7
Tensile Strength, Ultimate 23.0 - 49.0 MPa
3340 - 7110 psi
Average value: 38.2 MPa Grade Count:25
Tensile Strength, Yield 13.0 - 65.0 MPa
1890 - 9430 psi
Average value: 41.4 MPa Grade Count:92
22.1 - 59.3 MPa

@Temperature -18.0 - 71.0 °C
3210 - 8600 psi

@Temperature -0.400 - 160 °F
Average value: 40.7 MPa Grade Count:1
Elongation at Break 3.00 - 150 %
3.00 - 150 %
Average value: 34.3 % Grade Count:58
Elongation at Yield 0.620 - 70.0 %
0.620 - 70.0 %
Average value: 7.43 % Grade Count:44
Modulus of Elasticity 1.00 - 2.65 GPa
145 - 384 ksi
Average value: 2.09 GPa Grade Count:40
1.50 - 2.60 GPa

@Temperature -18.0 - 71.0 °C
218 - 377 ksi

@Temperature -0.400 - 160 °F
Average value: 2.05 GPa Grade Count:1
Flexural Yield Strength 28.3 - 88.3 MPa
4100 - 12800 psi
Average value: 63.9 MPa Grade Count:60
49.6 - 113.8 MPa

@Temperature -40.0 - 71.0 °C
7190 - 16510 psi

@Temperature -40.0 - 160 °F
Average value: 81.7 MPa Grade Count:1
Flexural Modulus 0.200 - 5.50 GPa
29.0 - 798 ksi
Average value: 2.20 GPa Grade Count:88
1.90 - 2.80 GPa

@Temperature -40.0 - 71.0 °C
276 - 406 ksi

@Temperature -40.0 - 160 °F
Average value: 2.35 GPa Grade Count:1
Izod Impact, Notched 0.380 - 10.3 J/cm
0.712 - 19.3 ft-lb/in
Average value: 3.26 J/cm Grade Count:77
0.450 - 3.00 J/cm

@Temperature -17.8 - 0.000 °C
0.843 - 5.62 ft-lb/in

@Temperature 0.000 - 32.0 °F
Average value: 1.28 J/cm Grade Count:11
0.480 - 4.00 J/cm

@Temperature -40.0 - 0.000 °C
0.899 - 7.49 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.28 J/cm Grade Count:13
0.480 - 4.00 J/cm

@Thickness 3.17 - 6.40 mm
0.899 - 7.49 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 1.28 J/cm Grade Count:13
Izod Impact, Unnotched 1.07873 - 1.66713 J/cm

@Temperature -20.0 - -20.0 °C
2.02091 - 3.12322 ft-lb/in

@Temperature -4.00 - -4.00 °F
Average value: 1.37 J/cm Grade Count:2
1.07873 - 1.66713 J/cm

@Thickness 3.20 - 6.40 mm
2.02091 - 3.12322 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 1.37 J/cm Grade Count:2
Izod Impact, Notched (ISO) 8.00 - 42.0 kJ/m²
3.81 - 20.0 ft-lb/in²
Average value: 26.4 kJ/m² Grade Count:16
7.00 - 22.0 kJ/m²

@Temperature -30.0 - -20.0 °C
3.33 - 10.5 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 13.1 kJ/m² Grade Count:10
7.00 - 7.00 kJ/m²

@Temperature -40.0 - -40.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 13.1 kJ/m² Grade Count:1
7.00 - 7.00 kJ/m²

@Thickness 4.00 - 4.00 mm
3.33 - 3.33 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 13.1 kJ/m² Grade Count:1
Charpy Impact Unnotched 11.0 J/cm² - NB
52.4 ft-lb/in² - NB
Average value: 14.6 J/cm² Grade Count:14
1.00 J/cm² - NB

@Temperature -40.0 - -30.0 °C
4.76 ft-lb/in² - NB

@Temperature -40.0 - -22.0 °F
Average value: 6.79 J/cm² Grade Count:15
Charpy Impact, Notched 0.900 - 5.00 J/cm²
4.28 - 23.8 ft-lb/in²
Average value: 2.57 J/cm² Grade Count:19
0.500 - 2.50 J/cm²

@Temperature -30.0 - -20.0 °C
2.38 - 11.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 1.49 J/cm² Grade Count:13
Thermal Properties Metric English Comments
CTE, linear 68.0 - 110 µm/m-°C
37.8 - 61.1 µin/in-°F
Average value: 87.8 µm/m-°C Grade Count:28
CTE, linear, Transverse to Flow 87.0 - 98.0 µm/m-°C
48.3 - 54.4 µin/in-°F
Average value: 93.7 µm/m-°C Grade Count:3
Thermal Conductivity 0.150 - 0.200 W/m-K
1.04 - 1.39 BTU-in/hr-ft²-°F
Average value: 0.172 W/m-K Grade Count:4
Maximum Service Temperature, Air 60.0 - 100 °C
140 - 212 °F
Average value: 84.3 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 107 °C
158 - 225 °F
Average value: 94.4 °C Grade Count:36
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 106 °C
158 - 223 °F
Average value: 89.0 °C Grade Count:82
Vicat Softening Point 88.0 - 125 °C
190 - 257 °F
Average value: 100 °C Grade Count:84
Glass Transition Temp, Tg 108 - 109 °C
226 - 228 °F
Average value: 108 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 - 1.00e+17 ohm-cm
1.00e+9 - 1.00e+17 ohm-cm
Average value: 7.17e+15 ohm-cm Grade Count:24
Surface Resistance 1.00e+9 - 1.00e+16 ohm
1.00e+9 - 1.00e+16 ohm
Average value: 1.03e+15 ohm Grade Count:24
Dielectric Constant 2.60 - 3.30
2.60 - 3.30
Average value: 2.99 Grade Count:10
Dielectric Strength 18.0 - 50.0 kV/mm
457 - 1270 kV/in
Average value: 33.2 kV/mm Grade Count:16
Dissipation Factor 0.00500 - 0.0200
0.00500 - 0.0200
Average value: 0.00886 Grade Count:9
Comparative Tracking Index 525 - 600 V
525 - 600 V
Average value: 588 V Grade Count:13
Hot Wire Ignition, HWI 7.00 - 60.0 sec
7.00 - 60.0 sec
Average value: 20.9 sec Grade Count:3
High Amp Arc Ignition, HAI 120 - 200 arcs
120 - 200 arcs
Average value: 136 arcs Grade Count:3
High Voltage Arc-Tracking Rate, HVTR 0.000 - 25.4 mm/min
0.000 - 1.00 in/min
Average value: 11.8 mm/min Grade Count:3
Users viewing this material also viewed the following: