Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.00 - 16.0 kJ/m²
3.81 - 7.61 ft-lb/in²
Average value: 10.7 kJ/m² Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Izod Impact, Notched (ISO) 6.00 - 16.0 kJ/m²
2.86 - 7.61 ft-lb/in²
Average value: 8.14 kJ/m² Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched (ISO) 14.0 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 17.5 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 14.0 - 16.0 kJ/m²

@Thickness 3.20 - 3.20 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 17.5 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 12.0 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.71 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 13.4 kJ/m² Grade Count:17
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 12.0 - 16.0 kJ/m²

@Thickness 3.20 - 3.20 mm
5.71 - 7.61 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 13.4 kJ/m² Grade Count:17
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 3.80 - 16.0 kJ/m²
1.81 - 7.61 ft-lb/in²
Average value: 7.07 kJ/m² Grade Count:7
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Izod Impact, Notched (ISO) 8.00 - 16.0 kJ/m²
3.81 - 7.61 ft-lb/in²
Average value: 10.9 kJ/m² Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Izod Impact, Notched (ISO) 2.00 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.25 kJ/m² Grade Count:24
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Notched (ISO) 2.40 - 16.0 kJ/m²
1.14 - 7.61 ft-lb/in²
Average value: 5.97 kJ/m² Grade Count:55
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 6.00 - 16.0 kJ/m²
2.86 - 7.61 ft-lb/in²
Average value: 10.2 kJ/m² Grade Count:5
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Izod Impact, Notched (ISO) 3.50 - 16.0 kJ/m²
1.67 - 7.61 ft-lb/in²
Average value: 8.10 kJ/m² Grade Count:55
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Izod Impact, Notched (ISO) 1.60 - 16.0 kJ/m²
0.761 - 7.61 ft-lb/in²
Average value: 6.02 kJ/m² Grade Count:33
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Notched (ISO) 2.60 - 16.0 kJ/m²
1.24 - 7.61 ft-lb/in²
Average value: 5.20 kJ/m² Grade Count:31
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 12.0 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.71 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 15.1 kJ/m² Grade Count:36
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched (ISO) 12.0 - 16.0 kJ/m²

@Thickness 3.20 - 3.20 mm
5.71 - 7.61 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 15.1 kJ/m² Grade Count:36
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched (ISO) 4.00 - 16.0 kJ/m²

@Temperature -30.0 - -18.0 °C
1.90 - 7.61 ft-lb/in²

@Temperature -22.0 - -0.400 °F
Average value: 8.77 kJ/m² Grade Count:39
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 6.50 - 16.0 kJ/m²
3.09 - 7.61 ft-lb/in²
Average value: 11.0 kJ/m² Grade Count:4
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Izod Impact, Notched (ISO) 4.60 - 16.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.19 - 7.61 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 8.37 kJ/m² Grade Count:15
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..