Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.70 - 4.70 kJ/m²

@Temperature -40.0 - -40.0 °C
1.76 - 2.24 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 4.03 kJ/m² Grade Count:4
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..