Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.70 - 13.0 kJ/m²
1.76 - 6.19 ft-lb/in²
Average value: 10.1 kJ/m² Grade Count:20
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Izod Impact, Notched (ISO) 3.70 kJ/m²

@Temperature 23.0 °C
1.76 ft-lb/in²

@Temperature 73.4 °F
ASTM D256
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled  (discontinued **)
Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications.
Izod Impact, Notched (ISO) 3.70 - 17.0 kJ/m²
1.76 - 8.09 ft-lb/in²
Average value: 11.3 kJ/m² Grade Count:11
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 3.70 kJ/m²
1.76 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY
Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a..
Izod Impact, Notched (ISO) >= 3.70 kJ/m²
>= 1.76 ft-lb/in²
DIN 53453
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Dry
Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 3.70 kJ/m²
1.76 ft-lb/in²
ISO 180
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced
20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 3.70 kJ/m²
1.76 ft-lb/in²
ISO 180
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Izod Impact, Notched (ISO) 3.70 kJ/m²
1.76 ft-lb/in²
ISO 180/1A
A.D. Compound Adene NCHA Homopolymer 25% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Notched (ISO) 3.70 - 4.70 kJ/m²

@Temperature -40.0 - -40.0 °C
1.76 - 2.24 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 4.03 kJ/m² Grade Count:4
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..