Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.00 - 90.0 kJ/m²
3.81 - 42.8 ft-lb/in²
Average value: 31.0 kJ/m² Grade Count:4
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 80.0 - 90.0 kJ/m²
38.1 - 42.8 ft-lb/in²
Average value: 82.5 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched (ISO) 8.00 - 90.0 kJ/m²

@Temperature -40.0 - -20.0 °C
3.81 - 42.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 24.1 kJ/m² Grade Count:52
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched (ISO) 8.00 - 90.0 kJ/m²
3.81 - 42.8 ft-lb/in²
Average value: 71.6 kJ/m² Grade Count:85
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..