Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.00 - 57.0 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 27.1 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 17.3 kJ/m² Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Izod Impact, Notched (ISO) 8.50 - 57.0 kJ/m²
4.04 - 27.1 ft-lb/in²
Average value: 18.0 kJ/m² Grade Count:10
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Izod Impact, Notched (ISO) 2.00 - 57.0 kJ/m²
0.952 - 27.1 ft-lb/in²
Average value: 17.5 kJ/m² Grade Count:63
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..