Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® XHT1143 PC (Asia Pacific) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR30 NL IH PA 6.6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® Rx1851 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 MR25 NL IL PA 6 25% mineral reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LG Chemical HF-380 ABS, High Flow, High Impact Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem |