Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Sax Polymers
Trade Name SAXAMID
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows high mechanical strength over a long period and is able to perform at higher temperatures.Information provided by SAX Polymers
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Viscosity Test 150 cm³/g
150 cm³/g
H<sub>2</sub>SO<sub>4</sub>; ISO 307
Mechanical Properties Metric English Comments
Tensile Strength 195 MPa
28300 psi
5 mm/min; ISO 527-1
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527-1
Tensile Modulus 9.80 GPa
1420 ksi
1 mm/min; ISO 527-1
Flexural Strength 280 MPa
40600 psi
2 mm/min; ISO 178
Flexural Modulus 8.00 GPa
1160 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 68.0 kJ/m²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 248 °C
478 °F
80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 255 °C
491 °F
B/120; ISO 306
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C

@Time 7200 - 21600 sec
176 °F

@Time 2.00 - 6.00 hour
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: