Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical HF-350 ABS, High Flow, High Impact Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 680 LNS503 High Performance Injection Molding Grade Lustran® ABS 680 LNS503 is an easy flow version. It is a high performance injection molding grade used for refrigerator and freezer door end caps. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Novodur® 4000PG ABS Novodur Ultra 4000PG is an injection molding grade especially suitable for electroplating, providing enhanced heat resistance.Information provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Styrolution Novodur® P2M-AT ABS Pellets Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -10.0 °C |
10.9 ft-lb/in² @Temperature 14.0 °F |
ISO 180 |
Dow INSPIRE™ 112 Performance Polymer INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion .. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |