Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering properties characterized by high strength; rigidity; good toughness; high melt point; good surface lubricity; abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline. Vydyne 21SPF BLK resin permits production of molded parts with good initial color plus good property and color retention when using regrind. This resin is recognized by Underwriters Laboratories and conforms to the requirements of many industrial, federal and military specifications for premium-quality, general-purpose PA66 resins. Vydyne 21SPF BLK resin is internally and externally lubricated for improved machine feed and exceptional mold release. In many applications, the molding cycle can be reduced because parts may be removed from the cavity at higher temperatures. In difficult molds where parts have a tendency to stick in the cavity. Vydyne 21SPF BLK can reduce or eliminate the need for mold release sprays. Critical molded part dimensions should be checked against specifications before implementing shorter molding cycles on a routine production basis. Availability:Asia PacificEuropeNorth America Additive:Lubricant Features:Fast Molding CycleGasoline ResistanceGood Abrasion ResistanceGood Chemical ResistanceGood Mold Release Good ToughnessHigh RigidityHigh StrengthLubricated Oil ResistantSolvent ResistantUses: BearingsBushingsCamsConnectorsElectrical Housings Industrial ApplicationsAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm

@Diameter 2.00 mm
0.020 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Diameter 2.00 mm
0.020 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-2
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Elongation at Yield 20 %
20 %
ISO 527-2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-2
Flexural Strength 30.0 MPa
4350 psi
ISO 178
Flexural Modulus 1.05 GPa
152 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180
23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA