Polymer Property : Izod Impact, Notched (ISO) = 3.70 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.70 kJ/m²

@Temperature 23.0 °C
1.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-1240 42% Chalk-Filled Polypropylene Homopolymer
INNOPOL® CS 1-1240 is a 42% chalk –filled polypropylene homopolymer compound /PP-H KD42 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1240 is devel..
Izod Impact, Notched (ISO) 3.70 kJ/m²

@Temperature -40.0 °C
1.76 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi..
Izod Impact, Notched (ISO) 3.70 kJ/m²

@Temperature 23.0 °C
1.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Hostacomâ„¢ BC142/1AC Polypropylene Copolymer
Description: Hostacomâ„¢ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It..
Izod Impact, Notched (ISO) 3.70 kJ/m²

@Temperature -30.0 °C
1.76 ft-lb/in²

@Temperature -22.0 °F
ISO 180
LyondellBasell Hostacom™ ZG750 Polypropylene Copolymer
Description: Hostacom™ ZG750 conventional melt flow, 1,700 MPa flexural modulus, 40% calcium carbonate-filled, utility grade polypropylene copolymer resin has a very good combination of strength, s..