LyondellBasell Hostacomâ„¢ BC142/1AC Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ BC142/1AC Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacomâ„¢ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It was designed primarily for structural automotive interior components that require high rigidity and low odor. Uses: Automotive interior partsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ISO 2039-2
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-1, -2
Elongation at Break 70 %
70 %
ISO 527-1, -2
Elongation at Yield 6.0 %
6.0 %
ISO 527-1, -2
Flexural Modulus 3.60 GPa
522 ksi
ISO 178
Izod Impact, Notched (ISO) 1.70 kJ/m²

@Temperature -40.0 °C
0.809 ft-lb/in²

@Temperature -40.0 °F
ISO 180
2.70 kJ/m²

@Temperature 10.0 °C
1.28 ft-lb/in²

@Temperature 50.0 °F
ISO 180
3.70 kJ/m²

@Temperature 23.0 °C
1.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
259 °F
Unannealed; ISO 75B-1, -2
Shrinkage 0.80 %
0.80 %
Tool, 100x150x3.2 mm; Basell Test Method