Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 71.0 MPa @Temperature 90.0 °C |
10300 psi @Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |
|||
Tensile Strength at Break | 71.0 MPa @Temperature 100 °C |
10300 psi @Temperature 212 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66
(Unverified Data**) Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im.. |