Polymer Property : Tensile Strength at Break = 71.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 71.0 MPa

@Temperature 90.0 °C
10300 psi

@Temperature 194 °F
ISO 527
DuPont Performance Polymers Rynite® 408 BK515 PET
Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info..
Tensile Strength at Break 71.0 MPa

@Temperature 100 °C
10300 psi

@Temperature 212 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66  (Unverified Data**)
Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im..