Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 25.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa

@Temperature 120 °C
3630 psi

@Temperature 248 °F
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Tensile Strength at Break 25.0 MPa

@Temperature 150 °C
3630 psi

@Temperature 302 °F
LATI Larpeek 10 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Strength at Break 25.0 MPa

@Temperature 90.0 °C
3630 psi

@Temperature 194 °F
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Strength at Break 25.0 MPa

@Temperature 23.0 °C
3630 psi

@Temperature 73.4 °F
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Tensile Strength at Break 25.0 MPa

@Temperature 23.0 °C
3630 psi

@Temperature 73.4 °F
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle..
Tensile Strength at Break 25.0 MPa

@Temperature 120 °C
3630 psi

@Temperature 248 °F
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Tensile Strength at Break 25.0 MPa

@Temperature 120 °C
3630 psi

@Temperature 248 °F
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Tensile Strength at Break 25.0 MPa

@Temperature 150 °C
3630 psi

@Temperature 302 °F
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Strength at Break 25.0 MPa

@Temperature 120 °C
3630 psi

@Temperature 248 °F
LATI Laril 13 G/20 PPOm, 20% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Strength at Break 25.0 MPa

@Temperature 60.0 °C
3630 psi

@Temperature 140 °F
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Strength at Break 25.0 MPa

@Temperature 120 °C
3630 psi

@Temperature 248 °F
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Strength at Break 25.0 MPa

@Temperature 150 °C
3630 psi

@Temperature 302 °F
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Strength at Break 25.0 MPa

@Temperature 60.0 °C
3630 psi

@Temperature 140 °F
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Strength at Break 25.0 MPa

@Temperature 90.0 °C
3630 psi

@Temperature 194 °F
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Carbon fiber. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Strength at Break 25.0 MPa

@Temperature 23.0 °C
3630 psi

@Temperature 73.4 °F
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Strength at Break 25.0 MPa

@Temperature 60.0 °C
3630 psi

@Temperature 140 °F
LATI Later 4-V0HF1 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Strength at Break 25.0 MPa

@Temperature 90.0 °C
3630 psi

@Temperature 194 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Tensile Strength at Break 25.0 MPa

@Temperature 60.0 °C
3630 psi

@Temperature 140 °F
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
Tensile Strength at Break 25.0 MPa

@Temperature 0.000 °C
3630 psi

@Temperature 32.0 °F
ASTM D638
Borealis Borstar® HE6081 Black Track Resistant HD Polyethylene Based Compound for Jacketing of Fiber Optical Cable
Borstar HE6081 is based on high-density polyethylene and has a specially designed additive package to give excellent track resistance. It is also well protected against UV degradation in order to e..
Tensile Strength at Break 25.0 MPa

@Temperature -30.0 °C
3630 psi

@Temperature -22.0 °F
ASTM D638
Borealis Borstar® HE6081 Black Track Resistant HD Polyethylene Based Compound for Jacketing of Fiber Optical Cable
Borstar HE6081 is based on high-density polyethylene and has a specially designed additive package to give excellent track resistance. It is also well protected against UV degradation in order to e..
Tensile Strength at Break 25.0 MPa

@Temperature 90.0 °C
3630 psi

@Temperature 194 °F
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Tensile Strength at Break 25.0 MPa

@Temperature 120 °C
3630 psi

@Temperature 248 °F
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; La..
Tensile Strength at Break 25.0 MPa

@Temperature 150 °C
3630 psi

@Temperature 302 °F
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Tensile Strength at Break 25.0 MPa

@Temperature 275 °C
3630 psi

@Temperature 527 °F
ISO 527
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..