Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)
Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 215 MPa

@Temperature 120 °C
31200 psi

@Temperature 248 °F
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 215 MPa

@Temperature 90.0 °C
31200 psi

@Temperature 194 °F
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 215 MPa

@Temperature 60.0 °C
31200 psi

@Temperature 140 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..