Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
0.05 in/min; ASTM D790A
ExxonMobil AXO3BE3 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt fl..
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790
Braskem GF4950 HDPE Blow Molding Polyethylene Copolymer
HDPE GF4950 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high environmental stress cracking resistance and processability. It was..
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness...
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM-D790
Braskem HC7260LS-L HDPE Injection Molding Polyethylene
HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its..
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene
Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta..
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790A
Braskem H 604 Thermoforming & Extrusion Polypropylene Homopolymer
Transparent packaging for food; Flat and corrugated sheets for school and office folders.Information provided by Braskem.
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM-D790
Braskem HA7260 HDPE Injection Molding Polyethylene
HA7260 is a high-density polyethylene that was developed for injection molding. It is easy to process and has high productivity, high rigidity and hardness, and a good melt flow. Its narrow molar ma..
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene
Description: SHC7260 is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. The minimum biobased content of ..