Material Notes:
HA7260 is a high-density polyethylene that was developed for injection molding. It is easy to process and has high productivity, high rigidity and hardness, and a good melt flow. Its narrow molar mass distribution results in low warpage. Its applications include: pails, basins, toys, lids, thin-walled parts, and housewares.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM-D792
ESCR 100% Igepal® <= 4.0 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
<= 4.0 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM-D2240
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM-D638
Elongation at Yield 7.2 %
7.2 %
ASTM-D638
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM-D790
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM-D648
Vicat Softening Point 124 °C

@Load 1.02 kg
255 °F

@Load 2.25 lb
ASTM-D1525