Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus, 1% Secant = 232000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
ASTM D790A
SABIC PP 520L Polypropylene Homopolymer for Tubular Water Quenched Film
Product Description: PP 520L is specially developed for tubular water quenched blown film applications with a suitable dosage of slip and antiblock additives.Films produced using PP 520L will exhib..
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
ASTM D790A
SABIC PP 575P Polypropylene Homopolymer for Injection Molding
Product Description: PP 575P is specially developed for producing rigid injection molding articles for general purpose applications. It gives consistent processability and high gloss in the produc..
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
0.5 in/min; ASTM D790B
ExxonMobil PP4712E1 Polymer Grade for Oriented Film
Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo..
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
ASTM-D790
Braskem PH 0242 HOMO Polypropylene Homopolymer
PH 0242 is a low melt flow rate homopolymer produced by compression molding. This resin exhibits excellent processability and excellent stiffness/impact strength balance. Its applications include co..
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
ASTM-D790
Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer
CP 202XP is a high melt flow rate heterophasic copolymer designed to achieve parts with high stiffness and impact strength resistance, low warpage, and excellent surface appearance. Its applications..