Polymer Property : K (wear) Factor = 21.0 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific)
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Dry: 0.25 m/s, 3.4 MPa (50 fpm, 500 psi); ASTM D3702
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC
LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK
LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK
LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP VERTON RVL29 PA 66
LNP VERTON* RVL29 is a compound based on Nylon 66 resin containing 45% Long Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Structural.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP VERTON RVL29 PA 66 (Asia Pacific)
LNP VERTON* RVL29 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Easy Molding.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
TriStar TriSteel AC Metal Backed PTFE Bearing System
Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate..
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP VERTON RVL29ESS PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RVL29ESS is a compound based on PA 66 resin, containing Long Glass Fiber, PTFE. Added features include; Internally Lubricated.
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP VERTON RVL29XXP PA 66 (Europe-Africa-Middle East)
LNP VERTON* RVL29XXP is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.