Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RVL29ESS PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RVL29ESS PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* RVL29ESS is a compound based on PA 66 resin, containing Long Glass Fiber, PTFE. Added features include; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 231 MPa
33500 psi
5 mm/min; ISO 527
Elongation at Break 2.3 %
2.3 %
5 mm/min; ISO 527
Flexural Yield Strength 362 MPa
52500 psi
2 mm/min; ISO 178
Flexural Modulus 14.1 GPa
2050 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1A
Coefficient of Friction, Dynamic 0.39
0.39
ASTM D3702 Modified
Coefficient of Friction, Static 0.40
0.40
ASTM D3702 Modified
K (wear) Factor 42.3 x 10-8 mm³/N-M
21.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 258 °C
496 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af