Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1055DE Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1090AE Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp..
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1095AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1190A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3085AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 5085A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1080AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1085A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3085A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tensile Strength, Yield 12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...