Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 30500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 210 MPa

@Strain 0.200 %,
Temperature 200 °C
30500 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4016 Ferritic Stainless Steel
Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su..
Tensile Strength, Yield 210 MPa

@Strain 0.200 %
30500 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 210 MPa

@Strain 0.200 %,
Temperature 100 °C
30500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel
Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro..
Tensile Strength, Yield 210 MPa

@Strain 0.200 %,
Temperature 400 °C
30500 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Yield >= 210 MPa

@Strain 0.200 %
>= 30500 psi

@Strain 0.200 %
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel
Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide prec..
Tensile Strength, Yield >= 210 MPa

@Strain 0.200 %
>= 30500 psi

@Strain 0.200 %
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL..
Tensile Strength, Yield 210.3 MPa

@Thickness 25.4 mm,
Temperature 427 °C
30500 psi

@Thickness 1.00 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'..