Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name CLC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide precipitations in grain boundaries. The grade contains some residual ferrite (=2%) after solution annealing (1100 - 1150°C/ 2012 - 2102°F) and water quenching. Its low carbon content avoids the intergranular corrosion, even on welded pieces without an ulterior water quenching. The high Molybdenum content gives this steel a higher resistance to corrosion in sulfuric media than standard grades (CLC17-12-2L / 316L). Its main properties are : high ductility, easy weldability and improved corrosion resistance. The main application are chemical tankers, chemical industries and pulp and paper industry.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 515 MPa
>= 74700 psi
Tensile Strength, Yield >= 210 MPa

@Strain 0.200 %
>= 30500 psi

@Strain 0.200 %
>= 250 MPa

@Strain 1.00 %
>= 36300 psi

@Strain 1.00 %
Elongation at Break >= 40 %
>= 40 %
Modulus of Elasticity 200 GPa

@Temperature 20.0 - 100 °C
29000 ksi

@Temperature 68.0 - 212 °F
Poissons Ratio 0.299
0.299
Calculated
Shear Modulus 77.0 GPa

@Temperature 20.0 - 100 °C
11200 ksi

@Temperature 68.0 - 212 °F
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.89 µin/in-°F

@Temperature 68.0 - 212 °F
16.5 µm/m-°C

@Temperature 20.0 - 200 °C
9.17 µin/in-°F

@Temperature 68.0 - 392 °F
17.0 µm/m-°C

@Temperature 20.0 - 300 °C
9.44 µin/in-°F

@Temperature 68.0 - 572 °F
18.0 µm/m-°C

@Temperature 20.0 - 500 °C
10.0 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C

@Temperature 20.0 - 100 °C
0.120 BTU/lb-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 14.0 W/m-K

@Temperature 20.0 - 100 °C
97.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 18.5 %
18.5 %
Iron, Fe 64.77 - 64.8 %
64.77 - 64.8 %
As remainder
Molybdenum, Mo 3.2 %
3.2 %
Nickel, Ni 13.5 %
13.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000750 ohm-cm

@Temperature 20.0 - 100 °C
0.0000750 ohm-cm

@Temperature 68.0 - 212 °F