Mechanical Properties Metric English Comments
Tensile Strength, Yield 460 MPa

@Strain 0.200 %
66700 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %
66700 psi

@Strain 0.200 %
hardened
Wieland Porta Aurium PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %
66700 psi

@Strain 0.200 %
hardened
Wieland Porta Maximum PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %,
Thickness 9.90 - 12.5 mm
>= 66700 psi

@Strain 0.200 %,
Thickness 0.390 - 0.492 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %,
Thickness 25.0 - 50.0 mm
>= 66700 psi

@Strain 0.200 %,
Thickness 0.984 - 1.97 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %,
Thickness 300 - 400 mm
66700 psi

@Strain 0.200 %,
Thickness 11.8 - 15.7 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %,
Thickness 400 - 450 mm
66700 psi

@Strain 0.200 %,
Thickness 15.7 - 17.7 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %,
Thickness 150 - 240 mm
66700 psi

@Strain 0.200 %,
Thickness 5.91 - 9.45 in
Typical Strength
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %,
Thickness 325 - 400 mm
66700 psi

@Strain 0.200 %,
Thickness 12.8 - 15.7 in
Typical Strength
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %,
Thickness 400 - 450 mm
66700 psi

@Strain 0.200 %,
Thickness 15.7 - 17.7 in
Typical Strength
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %,
Thickness 7.90 - 12.5 mm
>= 66700 psi

@Strain 0.200 %,
Thickness 0.311 - 0.492 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %,
Thickness 12.5 - 25.0 mm
>= 66700 psi

@Strain 0.200 %,
Thickness 0.492 - 0.984 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %,
Thickness 25.0 - 50.0 mm
>= 66700 psi

@Strain 0.200 %,
Thickness 0.984 - 1.97 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength, Yield 460 MPa

@Strain 0.200 %
66700 psi

@Strain 0.200 %
5% Cold Worked
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..
Tensile Strength, Yield >= 460 MPa

@Strain 0.200 %
>= 66700 psi

@Strain 0.200 %
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion..