Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 655 MPa

@Strain 0.200 %,
Thickness 12.7 - 25.4 mm
>= 95000 psi

@Strain 0.200 %,
Thickness 0.500 - 1.00 in
ASTM E-8
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate
Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength, Yield >= 655 MPa

@Strain 0.200 %,
Thickness <=0.0254 mm
>= 95000 psi

@Strain 0.200 %,
Thickness <=0.00100 in
ASTM E-345
H.C. Starck F-21-5 Pure Molybdenum, Foil
F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli..
Tensile Strength, Yield >= 655 MPa

@Strain 0.200 %,
Thickness 0.0254 - 0.0508 mm
>= 95000 psi

@Strain 0.200 %,
Thickness 0.00100 - 0.00200 in
ASTM E-345
H.C. Starck F-21-5 Pure Molybdenum, Foil
F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli..
Tensile Strength, Yield >= 655 MPa

@Strain 0.200 %,
Thickness 0.0508 - 0.0762 mm
>= 95000 psi

@Strain 0.200 %,
Thickness 0.00200 - 0.00300 in
ASTM E-345
H.C. Starck F-21-5 Pure Molybdenum, Foil
F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli..
Tensile Strength, Yield >= 655 MPa

@Strain 0.200 %,
Thickness 0.0762 - 0.124 mm
>= 95000 psi

@Strain 0.200 %,
Thickness 0.00300 - 0.00490 in
ASTM E-345
H.C. Starck F-21-5 Pure Molybdenum, Foil
F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli..
Tensile Strength, Yield >= 655 MPa

@Diameter 22.2 - 28.57 mm,
Strain 0.200 %
>= 95000 psi

@Diameter 0.875 - 1.125 in,
Strain 0.200 %
ASTM E-8
H.C. Starck Molybdenum Alloy PBT, Bar
Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg..
Tensile Strength, Yield >= 655 MPa

@Diameter 22.2 - 28.57 mm,
Strain 0.200 %
>= 95000 psi

@Diameter 0.875 - 1.125 in,
Strain 0.200 %
ASTM E-8
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar
Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma..
Tensile Strength, Yield 655 - 862 MPa

@Strain 0.200 %,
Thickness <=25.4 mm
95000 - 125000 psi

@Strain 0.200 %,
Thickness <=1.00 in
Cold Drawn Bar
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar
Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan..
Tensile Strength, Yield 655 MPa

@Thickness 25.4 mm
95000 psi

@Thickness 1.00 in
Longitudinal Direction
Alcoa 7055-T7751 Aluminum Plate
Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Crucible Steel 431 Chromium Steel
Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Crucible Steel 431 Chromium Steel
Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten..