Polymer Property : Limiting Pressure Velocity = 0.333 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.333 MPa-m/sec
9500 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col..
Limiting Pressure Velocity 0.333 MPa-m/sec
9500 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col..
Limiting Pressure Velocity 0.333 - 0.701 MPa-m/sec
9500 - 20000 psi-ft/min
Average value: 0.587 MPa-m/sec Grade Count:11
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Limiting Pressure Velocity 0.333 MPa-m/sec
9500 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Semitron® ESd 420- CM Dissipative Polyetherimide(ASTM Product Data Sheet)