Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0800 - 0.701 MPa-m/sec
2280 - 20000 psi-ft/min
Average value: 0.398 MPa-m/sec Grade Count:7
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
Limiting Pressure Velocity 0.333 - 0.701 MPa-m/sec
9500 - 20000 psi-ft/min
Average value: 0.587 MPa-m/sec Grade Count:11
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..