Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.380 MPa-m/sec | 10800 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Limiting Pressure Velocity | 0.380 - 12.0 MPa-m/sec | 10800 - 343000 psi-ft/min | Average value: 3.62 MPa-m/sec Grade Count:6 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |