Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.380 - 12.0 MPa-m/sec | 10800 - 343000 psi-ft/min | Average value: 3.62 MPa-m/sec Grade Count:6 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |