Limiting Pressure Velocity 0.380 MPa-m/sec
10800 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data)
Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good ..
Limiting Pressure Velocity 0.380 - 12.0 MPa-m/sec
10800 - 343000 psi-ft/min
Average value: 3.62 MPa-m/sec Grade Count:6
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..